Experimental work on possibilities to predict casting defects in LPDC brass castings

  • A. Muikku
  • , J. Hartikainen
  • , S. Vapalahti
  • , T. Tiainen

Research output: Contribution to journalArticleScientificpeer-review

5 Citations (Scopus)
Translated title of the contributionExperimental work on possibilities to predict casting defects in LPDC brass castings
Original languageEnglish
Pages (from-to)561-566
JournalMaterials Science Forum
Volume508
DOIs
Publication statusPublished - 2006