Mechanical Behavior of Superalloy MA 760 During High Temperature Cyclic Straining

  • A. Hynnä
  • , V.-T. Kuokkala
  • , P. Kettunen

    Research output: Chapter in Book/Report/Conference proceedingConference contributionScientific

    Translated title of the contributionMechanical Behavior of Superalloy MA 760 During High Temperature Cyclic Straining
    Original languageEnglish
    Title of host publicationProceedings of The Sixth International Fatigue Congress, Berlin 6.-10.5.1996
    EditorsG. Lütjering, H. Nowack
    Place of PublicationBerlin, Germany
    Pages825-830
    Publication statusPublished - 1996
    Publication typeB3 Article in conference proceedings

    Publication forum classification

    • No publication forum level

    Cite this