Novel high temperature vacuum nanoindentation system with active surface referencing and non-contact heating for measurements up to 800 °C

Marcello Conte, Gaurav Mohanty, Jakob J. Schwiedrzik, Jeffrey M. Wheeler, Bertrand Bellaton, Johann Michler, Nicholas X. Randall

Research output: Contribution to journalArticleScientificpeer-review

10 Citations (Scopus)
3 Downloads (Pure)

Fingerprint

Dive into the research topics of 'Novel high temperature vacuum nanoindentation system with active surface referencing and non-contact heating for measurements up to 800 °C'. Together they form a unique fingerprint.

Physics & Astronomy

Engineering & Materials Science