Protective Quality of Sputtered TiN Coatings on Superalloys

A. Telama, T. Mäntylä, P. Kettunen

    Research output: Book/ReportCommissioned report

    Translated title of the contributionProtective Quality of Sputtered TiN Coatings on Superalloys
    Original languageEnglish
    Place of PublicationTampere
    PublisherTampere University of Technology
    Publication statusPublished - 1986
    Publication typeD4 Published development or research report or study

    Publication series

    NameTampere University of Technology, Institute of Materials Science, Report
    PublisherTampere University of Technology
    No.25/1986