Fatique Properties of ODS Superalloy at High Temperatures

    Aktiviteetti: Konferenssiesitelmä

    Aikajakso1986
    Tapahtuman otsikkoFirst ASM Europe Technical Conference, Symposium on Advanced Materials and Pr ocessing Techniques for Structural Applications. 7-8 September 1986, Paris
    Tapahtuman tyyppiConference

    Country of activity

    • Ranska

    Publication forum classification

    • Ei tasoa