Abstrakti
The high-temperature corrosion of high velocity air-fuel (HVAF) thermal spray Ni21Cr, Ni5Al, and Ni21Cr7AlY coatings was investigated at 600 °C for 168 h in ambient air under KCl and 50-50 mol% KCl–K2SO4 salts. Chlorination-oxidation cycle and breakdown of the corrosion products layer were the dominant corrosion mechanism in the chromia-forming Ni21Cr and Ni21Cr7AlY coatings exposed to KCl. KCl–K2SO4 was less corrosive to the chromia-forming coatings as K2SO4 was less reactive to the protective Cr-rich oxide. The alumina-forming NiAl exhibited a better corrosion performance under KCl, though it partially suffered from selective sulfidation when exposed to the mixed salt.
| Alkuperäiskieli | Englanti |
|---|---|
| Artikkeli | 108066 |
| Sivumäärä | 19 |
| Julkaisu | Corrosion Science |
| Vuosikerta | 160 |
| DOI - pysyväislinkit | |
| Tila | Julkaistu - marrask. 2019 |
| Julkaistu ulkoisesti | Kyllä |
| OKM-julkaisutyyppi | A1 Alkuperäisartikkeli tieteellisessä aikakauslehdessä |
Sormenjälki
Sukella tutkimusaiheisiin 'High-temperature corrosion performance of HVAF-sprayed NiCr, NiAl, and NiCrAlY coatings with alkali sulfate/chloride exposed to ambient air'. Ne muodostavat yhdessä ainutlaatuisen sormenjäljen.Siteeraa tätä
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver