The Effect of Phosphorus Exposure on Diesel Oxidation Catalysts-Part I: Activity Measurements, Elementary and Surface Analyses

Marja Kärkkäinen, Tanja Kolli, Mari Honkanen, Olli Heikkinen, Mika Huuhtanen, Kauko Kallinen, Toivo Lepistö, Jouko Lahtinen, Minnamari Vippola, Riitta L. Keiski

    Tutkimustuotos: ArtikkeliTieteellinenvertaisarvioitu

    19 Sitaatiot (Scopus)

    Abstrakti

    The effects of phosphorus poisoning on the activity of PtPd and Pt diesel oxidation catalysts and on the activity of the support material were investigated using the gas phase laboratory-scale-aging procedure. The catalysts were treated using two different phosphorus concentrations (0.065 and 0.13 mol/L (NH4)(2)HPO). The deactivation was studied by inductively coupled plasma optical emission spectroscopy, electron microscopy, X-ray diffractometry, X-ray photoelectron spectrometry and Fourier-transform infrared reflectance, N-2-physisorption, and activity measurements with CO, C3H6 and NO. The amount of accumulated phosphorus was higher on the Pt catalyst surface than on the PtPd catalyst and significantly higher on the surface of the bare support material. Phosphorus concentration was uniform throughout the support layer (down to the 10 mu m), and phosphorus was found as phosphate, although it can also form compounds like AIPO(4) with the support. The treatment with low phosphorus concentration was found to have a clear deactivation effect only for C3H6 oxidation activity on PtPd catalysts above 200 degrees C. The treatment with high phosphorus concentration significantly decreased the activity of both the PtPd and Pt catalysts. In particular, the C3H6 and NO oxidation activities of the fresh and P-treated Pt catalysts were higher than those of the PtPd catalysts for the entire temperature range.

    AlkuperäiskieliEnglanti
    Sivut961-970
    Sivumäärä10
    JulkaisuTopics in Catalysis
    Vuosikerta58
    Numero14
    DOI - pysyväislinkit
    TilaJulkaistu - lokak. 2015
    OKM-julkaisutyyppiA1 Alkuperäisartikkeli tieteellisessä aikakauslehdessä

    Julkaisufoorumi-taso

    • Jufo-taso 1

    Sormenjälki

    Sukella tutkimusaiheisiin 'The Effect of Phosphorus Exposure on Diesel Oxidation Catalysts-Part I: Activity Measurements, Elementary and Surface Analyses'. Ne muodostavat yhdessä ainutlaatuisen sormenjäljen.

    Siteeraa tätä